Bare-to-Finish Solutions to Solve Paint Blistering on Exterior Walls & Floors

Choose a exterior surface to view our recommended full-system solutions

System Solutions for Paint Blistering on Floor

Over time, moisture buildup beneath the paint layer can cause blistering and lifting, especially in humid environments. Nippon Paint’s Bare-to-Finish Solution for Paint Blistering on Floors is designed to address the root cause and provide long-term protection, so you can enjoy a smooth, flawless finish in your most beautiful home.

5 Paint (Second Coat)
4 Paint (First Coat)
3 Primer
2 Sanding
1 Surface Preparation
1

Surface Preparation

Use a scraper to remove all loose paint film, then ensure the surface is clean, dry, and free of dust or debris.

5 Paint (Second Coat)
4 Paint (First Coat)
3 Primer
2 Sanding
1 Surface Preparation

2
Nippon Paint Abrasive Waterproof Sandpaper packaging featuring product details and usage instructions. Ideal for achieving smooth finishes on various surfaces, the sandpaper measures 230x280mm and is suitable for wood, metal, and plastic applications.

Sanding

Abrasive Waterproof Sandpaper

Lightly sand the surface to even out imperfections and ensure strong bonding for the next coating layers.


3
Nippon Paint EA9 Finish HB protective coatings in two cans, featuring high-performance and heavy-duty formulations. The larger can is the base, while the smaller can is the hardener for optimal mixing. Ideal for durable and long-lasting finishes.

Primer

EA9 Finish HB

Add a high-performance primer coat to protect the surface from rust, friction, and external damage over time.


4

Paint (First Coat)

Floorsports 1K Epoxy Hybrid

Apply a uniform layer of topcoat to enhance the flooring’s appearance while improving its resistance to daily wear and tear.


5

Paint (Second Coat)

Floorsports 1K Epoxy Hybrid

Apply a second topcoat to deepen the colour and strengthen protection, creating a more durable, water-resistant surface.

Achieving durable exterior walls through a compatible system 

From preparation to the final coat, every step in the exterior paint process matters. When these layers work in harmony, they strengthen adhesion, improve durability, and maintain a more consistent finish. Nippon Paint’s Bare-to-Finish Solution to Solve Paint Blistering on Exterior Floors guides homeowners towards better performance from start to finish. Discover from the Nippon Paint House Pakar why a proper start makes all the difference.

Your Guide to Bare-to-Finish Solutions for Paint Blistering

Learn all about how to solve your blistering paint problems at exterior areas.

What Causes Paint Blistering on Floors?

Blisters can form beneath the paint film when moisture, heat, or air becomes trapped, gradually causing the coating to lift from the surface. Nippon Paint’s Bare-to-Finish Solution helps restore adhesion and reduce the risk of recurring blistering.

Trapped moisture

Water from leaks, condensation, or high humidity can become trapped beneath the paint layer. When exposed to heat, the moisture expands into vapour, forming bubbles that lead to blistering.

Painting on a damp or hot surface

Applying paint on surfaces that are not fully dry or overheated by direct sunlight can trap moisture or solvents beneath the film, causing bubbles to form as they evaporate.

Incorrect paint or application method

Using the wrong paint type, applying coats too thickly, or re-coating before the previous layer has cured can prevent proper drying, resulting in blister formation.

The right steps and products can help prevent paint blistering on exterior floors. With a complete system designed to work together, Nippon Paint’s Bare-to-Finish Solution can eliminate existing blistering, reinforce the floor surface, and prevent future coating problems, ensuring a smooth, long-lasting, and visually appealing exterior finish.

Explore our recommended system solutions or speak to a Nippon Paint expert to find the right approach for your home.